RECEIVED by McKinney Cameron on date 5/25/2007 From RTI
ROC | ROC wafer | Label |
---|---|---|
ROC0 | KZNG1JT | 33B |
ROC1 | KZNG1JT | 62B |
ROC2 | KZNG1JT | 52B |
ROC3 | KZNG1JT | 62D |
ROC4 | KZNG1JT | 52D |
ROC5 | KZNG1JT | 73B |
ROC6 | KZNG1JT | 74B |
ROC7 | KZNG1JT | 54A |
ROC8 | KZNG1JT | 13A |
ROC9 | KZNG1JT | 54C |
Inspected by McKinney Cameron on date 5/25/2007
Picture | Comment |
---|---|
![]() | ROC1 is labeled 62B but is listed as 62A in the shipment file. |
![]() | Some debris between ROCs 1 and 2 |
![]() | Ring of dirt on the right side of ROC2 |
![]() | Circular spot of residue in the middle of ROC9 |
IV Measured by McKinney Cameron on date 5/25/2007
![]() | IV XML File |